Publication Laka-library:
General Corrosion and Stress Corrosion Cracking studies on Carbon Steels for Application in Nuclear Waste Disposal Containers (1993)
| Author | Smailos, Fiehn, Gago, Azkarate, KfK Karlsruhe |
| Date | March 1993 |
| Classification | 6.01.5.51/37 (WASTE - STORAGE ON LAND (f.i. SALT / CLAY) (INCL. SYNROC)) |
| Front | ![]() |
From the publication:
Summary In previous corrosion studies, carbon steels and the alloy Ti 99.8-Pd were identified as promising materials for heat-generating nuclear waste containers acting as a radionuclide barrier in a rock salt repository. To characterize the long-term corrosion behaviour of these materials in more detail, a research programme including laboratory-scale and in-situ corrosion studies has been undertaken jointly by KfK and ENRESA/INASMET. Besides carbon steels and Ti 99.8-Pd, also Hastelloy C4 and some selected Fe-base materials are being examined in order to complete the results available to date. In the period under review, the 18-month immersion experiments and the stress corrosion cracking studies (slow strain rate tests) on three preselected carbon steels in disposal relevant brines at 150°C-170 °C were completed. Moreover, first irradiation-corrosion studies were performed on the unalloyed carbon steel TSt E 355 in salt brines at 150°C and a realistic gamma dose rate of 10 Gy/h for thick-walled containers.
This publication is only available at Laka on paper, not as pdf.
You can borrow the publication or request a copy. When we're available, this is possible for a small fee.