General Corrosion and Stress Corrosion Cracking studies on Carbon Steels for Application in Nuclear Waste Disposal Containers (1993)

AuteurSmailos, Fiehn, Gago, Azkarate, KfK Karlsruhe
Datummaart 1993
Classificatie6.01.5.51/37 (AFVAL - OPSLAG OP LAND (oa ZOUT/KLEI))
Voorkant

Uit de publicatie:

Summary

In previous corrosion studies, carbon steels and the alloy Ti 99.8-Pd were identified
as promising materials for heat-generating nuclear waste containers acting as a
radionuclide barrier in a rock salt repository. To characterize the long-term corrosion
behaviour of these materials in more detail, a research programme including
laboratory-scale and in-situ corrosion studies has been undertaken jointly by KfK
and ENRESA/INASMET. Besides carbon steels and Ti 99.8-Pd, also Hastelloy C4
and some selected Fe-base materials are being examined in order to complete the
results available to date.

In the period under review, the 18-month immersion experiments and the stress
corrosion cracking studies (slow strain rate tests) on three preselected carbon
steels in disposal relevant brines at 150°C-170 °C were completed. Moreover, first
irradiation-corrosion studies were performed on the unalloyed carbon steel TSt E 355
in salt brines at 150°C and a realistic gamma dose rate of 10 Gy/h for thick-walled
containers.